Thermal Properties Metric English Comments
Minimum Service Temperature, Air -60.0 - -30.0 °C
-76.0 - -22.0 °F
Average value: -48.2 °C Grade Count:241
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Minimum Service Temperature, Air -65.0 - -30.0 °C
-85.0 - -22.0 °F
Average value: -52.0 °C Grade Count:48
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Minimum Service Temperature, Air -40.0 - -30.0 °C
-40.0 - -22.0 °F
SMAC SMACWRAP® EX Damping Material, 0.12 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Minimum Service Temperature, Air -40.0 - -30.0 °C
-40.0 - -22.0 °F
SMAC SMACWRAP® ST Damping Material, 0.10 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Minimum Service Temperature, Air -40.0 - -30.0 °C
-40.0 - -22.0 °F
SMAC SMACWRAP® ST Damping Material, 0.20 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Minimum Service Temperature, Air -40.0 - -30.0 °C
-40.0 - -22.0 °F
SMAC SMACWRAP® ST Damping Material, 0.60 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Minimum Service Temperature, Air -40.0 - -30.0 °C
-40.0 - -22.0 °F
SMAC SMACWRAP® ST Damping Material, 1 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Minimum Service Temperature, Air -40.0 - -30.0 °C
-40.0 - -22.0 °F
SMAC SMACWRAP® EX Damping Material, 0.20 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure without..