Polymer Property : Minimum Service Temperature, Air = -226 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -226 °C
-375 °F
Embrittlement Temp
TriStar Ultracomp UC-200 Composite Bearing
Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m..
Minimum Service Temperature, Air -226 °C
-375 °F
Embrittlement Temp
TriStar Ultracomp UC-300 Composite Bearing
Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family..