Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 173 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 795A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants PML-81 Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8170 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8170U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8172 (829) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Precision Polymer Engineering N65H Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content = 40% plus. Copolymer of acrylonitrile and butadiene.Applications: The high acrylonitrile content of this compound inc.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Precision Polymer Engineering N90L Nitrile Rubber Low Nitrile Rubber, 85-95 °IRHD. Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. ASTM D2000 line call-out M6BG907, A14, B.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70R Polyurethane Rubber Peroxide cured, red Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion r.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70W Polyurethane Rubber Peroxide cured, off-white Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abra.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70X Polyurethane Rubber Peroxide cured, self-lubricating, Polyurethane Rubber, 65-75 °IRHD. Compounded with graphite or molyb-d. To meet ASTM line call-out M5BG714, B14, EO14, EO34. Polyester-based urethane. ASTM & ISO d.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q75B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG728, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q80Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 75-85 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG814, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Freudenberg Simrit V115 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Freudenberg Simrit V123 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Retraction Temperature, TR10; ASTM D1329 |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | as heat transfer fluid |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B419 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B571 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B574 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg E850 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H608 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H711 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H730 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B870 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
ChevronTexaco CP Grease FeaturesChevron CP Grease is a corrosion preventive grease.It is manufactured with a special low viscosity, low pour point base oil, a lithium thickener, and rust and oxidation inhibitors. It is lig.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | See Note 1. |
ChevronTexaco MCP Grease L NLGI Grade 00 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | JIS-K-6723 |
Denka REOMER G G5379 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Brittleness Temperature |
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(disco Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |