Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -31.7 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -31.7 °C
-25.0 °F
Approx. Cold test
Lubriplate 1200-2 Lithium Type Multi-Purpose Grease
This is a heavy-duty general purpose lithium type grease for both industrial and automotive applications. It provides a high film strength, shear stability, and AW & EP additives. Applications: Gene..
Minimum Service Temperature, Air -31.7 °C
-25.0 °F
Approx. Cold test
Lubriplate SFL-2 Aluminum Complex Synthetic Food Machinery Grade Grease
This series provides an exceptionally wide operating temperature range, high shear stability, excellent water resistance, and load carrying properties. For use in freezers and other cold temperature..
Copyright © lookpolymers.com All Rights Reserved