Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -196 °C | -320 °F | |
Polygon Polylube™ Fiber Series Epoxy Composite Bearings Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bea.. |
|||
Minimum Service Temperature, Air | -196 °C | -320 °F | |
Saint-Gobain Rulon® CJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |
|||
Minimum Service Temperature, Air | -196 °C | -320 °F | |
TriStar CJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
Minimum Service Temperature, Air | -196 °C | -320 °F | |
TriStar FCJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
Minimum Service Temperature, Air | -196 °C | -320 °F | |
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |