Polymer Property : Minimum Service Temperature, Air = -41.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -41.0 °C
-41.8 °F
Gehman T100
Zeon Chemicals HyTemp® 4054 AR Polyacrylate Elastomer
HyTemp 4054 contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent low temperature, heat and compression set with good oil resistence.Mo..
Minimum Service Temperature, Air -41.0 °C
-41.8 °F
Gehman T100
Zeon Chemicals HyTemp® 4454 AR Polyacrylate Elastomer
HyTemp 4454 is a ground form of HyTemp 4054, which contains one or more acrylic esters with a small percentage of a carboxy/chlorine cure site.Particulate version of HyTemp 4054.