Minimum Service Temperature, Air -43.0 °C
-45.4 °F
JIS-K-6723
Denka LCS Z1060 Thermoplastic Elastomer, Extrusion grade (general)
"DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r..
Minimum Service Temperature, Air -43.0 °C
-45.4 °F
JIS-K-6723
Denka REOMER G G5072 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -43.0 °C
-45.4 °F
JIS-K-6723
Denka VINYKON G5070 PVC, W grade for non-migratory sheath and special items
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..