Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -200 - -50.0 °C | -328 - -58.0 °F | Average value: -117 °C Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Minimum Service Temperature, Air | -260 - -50.0 °C | -436 - -58.0 °F | Average value: -131 °C Grade Count:10 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
Minimum Service Temperature, Air | -260 - -50.0 °C | -436 - -58.0 °F | Average value: -161 °C Grade Count:15 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |