Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -57.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
TR10
Precision Polymer Engineering F60A Fluorosilicone Rubber
Blue Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 60...
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
TR10
Precision Polymer Engineering F70A Fluorosilicone Rubber
Blue Fluorosilicone Rubber, 60 to 70 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, ..
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
TR10
Precision Polymer Engineering F80X Fluorosilicone Rubber
Mid-Blue Fluorosilicone Rubber, 76-85 °IRHD . Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1,..
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
Silicone Version
Parker Chomerics POLASTRIP® Metal EMI Gasket
Description: POLASTRIP gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASTRIP gasketing, EMI shieldin..
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
Brittleness Temperature
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
Brittleness Temperature
DuPont Performance Polymers Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound &n
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
Dow Corning 4 ELECTRICAL INSULATING COMPOUND
Silicone-based compound, moderate consistency. Lubricant suitable for electrical connectors and joints.Information provided by Dow Corning
Copyright © lookpolymers.com All Rights Reserved