Polymer Property : Minimum Service Temperature, Air = -7.60 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -22.0 °C
-7.60 °F
Flexibility Fail Temperature; Huntsman Method
REXtac Rextac® RT 3280 Amorphous Polyalphaolefin (APAO)
Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Temperature resistance, high melt viscosity, and hardnessApplications: Component of modified bitumen roofing..
Minimum Service Temperature, Air -22.0 °C
-7.60 °F
TR test, TR70
Daikin DAI-EL LT-302 Fluoroelastomer, Low Temperature Grade, 64% Fluorine Content
Features: Flexible up to -30°C, excellent low temperature sealing.Information provided by Daikin Industries.
Minimum Service Temperature, Air -22.0 °C
-7.60 °F
JIS-K-6723
Denka VINYKON S210040 PVC, S grade for transparent extrusion molding
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Minimum Service Temperature, Air -22.0 °C
-7.60 °F
JIS-K-6723
Denka VINYKON W7080 PVC, W grade for non-migratory sheath and special items
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..