Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -45.6 - -17.8 °C | -50.0 - 0.000 °F | Average value: -28.9 °C Grade Count:29 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |