Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -6.00 °C | 21.2 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent compression set.Information provided by.. |
|||
Minimum Service Temperature, Air | -6.00 °C | 21.2 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-751 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent metal bonding and compression set.Infor.. |
|||
Minimum Service Temperature, Air | -6.00 °C | 21.2 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |