Thermal Properties Metric English Comments
Minimum Service Temperature, Air -60.0 - -3.40 °C
-76.0 - 25.9 °F
Average value: -37.1 °C Grade Count:32
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..