Minimum Service Temperature, Air 170 °C
338 °F
Synergy Polymers Ultra Purge P-O
Ultra Purge is a specially designed cleaning compound that comes premixed and ready-to-use in pellet form. It cleans black specks and deposits from screws, barrels, nozzle, hot runners and heads of ..