Polymer Property : Minimum Service Temperature, Air = 59.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 15.0 °C
59.0 °F
Henkel Frekote Aqualine C-800 Mold Release Agent
A water-based, zero VOC, mold release designed for releasing composite materials. This product offers easy application and higher number of releases which causes lower product usage and less operato..
Minimum Service Temperature, Air 15.0 °C
59.0 °F
Henkel Frekote PMC Mold Solvent
PMC is a special blend of solvents designed to dissolve and remove wax from molds without dulling the surface. This product can also be used to clean composite and metal mold surfaces as well as for..
Minimum Service Temperature, Air 15.0 °C
59.0 °F
Cured surfaces
3M Controltac™ 3552C Changeable Graphic Film with Comply™ Adhesive
2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to surfaces with corrugations and rivets; Air release channels for fast, easy, bub..
Minimum Service Temperature, Air 15.0 °C
59.0 °F
Cured surfaces
3M Controltac™ 8652C Changeable Graphic Film with Comply™ Adhesive
Film 8652C is a 2-mil film with sideable, repositionable, pressure-activated adhesive. This short-term durable and removable film is an excellent choice for fleet graphics, including surfaces with c..
Minimum Service Temperature, Air 15.0 °C
59.0 °F
Cured surfaces
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive
2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu..
Minimum Service Temperature, Air 15.0 °C
59.0 °F
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape
Scotch® Heavy Duty Vinyl Electrical Tape 22 is a premium grade, 10 mil thick, vinyl chloride tape. It is designed to perform continuously in ambient temperatures up to 80°C. The tape is conformabl..