Polymer Property : Heat of Fusion = 14.2 BTU/lb
Polymer Property :
Heat of Fusion =
14.2 BTU/lb
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Heat of Fusion
33.0
J/g
14.2
BTU/lb
ASTM D3417
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA)
Information provided by Arkema Group