POLYMER SEARCH
Polymer Property : Heat of Fusion = 14.40 BTU/lb
Polymer Property :
Heat of Fusion =
14.40 BTU/lb
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Heat of Fusion
33.47
J/g
14.40
BTU/lb
DOWM 100789-LE90A
Dow Tyrin® CM674 Elastomer Formulation
FormulationTyrin® CPE Elastomer