Thermal Properties Metric English Comments
Heat of Fusion 41.0 J/g
17.6 BTU/lb
Crystallinity; ExxonMobil Method
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin
Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Heat of Fusion 41.0 - 50.0 J/g
17.6 - 21.5 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.
Copyright © lookpolymers.com All Rights Reserved