Thermal Properties Metric English Comments
Heat of Fusion 23.0 J/g
9.89 BTU/lb
80°C to end of melting
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer  (discontinued **)
Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P..
Heat of Fusion 23.0 - 29.0 J/g
9.89 - 12.5 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.
Heat of Fusion 23.0 J/g
9.89 BTU/lb
80°C to end of melting
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer  (discontinued **)
Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..