Polymer Property : Heat of Fusion = 23.7 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 55.0 - 65.0 J/g
23.7 - 28.0 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers.