Polymer Property : Heat of Fusion = 5.00 J/g
Polymer Property :
Heat of Fusion =
5.00 J/g
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Heat of Fusion
5.00
J/g
2.15
BTU/lb
ASTM D3417
Arkema Group Pebax® 2533 Polyether Block Amide (PEBA)
Information provided by Arkema Group