Polymer Property : CTE, linear, Parallel to Flow = 1.00 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 1.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
0.556 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f..
CTE, linear, Parallel to Flow 1.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.556 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC
LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan..
CTE, linear, Parallel to Flow 1.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.556 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Stat-kon TE002
LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..
CTE, linear, Parallel to Flow 1.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.556 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON TE002 PU
LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
CTE, linear, Parallel to Flow 1.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.556 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC
LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
CTE, linear, Parallel to Flow 1.00 - 5.00 µm/m-°C

@Temperature 20.0 °C
0.556 - 2.78 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,..