Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl..
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MX05038 PP (Europe-Africa-Middle East)
Polypropylene compound, containing miniral. Added features include High ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East)
LNP *THERMOCOMP* PB006EQ is a compound based on PA 6 containing Glass Bead. Added features include Reduced Moisture.
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starpylen MX05038 TPEX, Injection Molded
Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON PX05047 PA 6 (Europe-Africa-Middle East)
LNP* Stat-kon* PX05047 is a compound based on PA 6 resin containing Carbon Fiber, Proprietary Filler (s). Added features include: Electrically Conductive, High Impact.
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 26.0 - 200 °C
60.6 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material
Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings Information ..