Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 - 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 - 66.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
BASF Ultramid® Seal-Fit PA6/66 (Dry)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
CTE, linear, Parallel to Flow 30.0 - 120 µm/m-°C

@Temperature 23.0 - 80.0 °C
16.7 - 66.7 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT
Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so..