Polymer Property : CTE, linear, Parallel to Flow = 15.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.4 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66
LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant.