Polymer Property : CTE, linear, Parallel to Flow = 150 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 - 150 µm/m-°C

@Temperature 0.000 - 40.0 °C
72.2 - 83.3 µin/in-°F

@Temperature 32.0 - 104 °F
1
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
CTE, linear, Parallel to Flow 130 - 150 µm/m-°C

@Temperature 0.000 - 40.0 °C
72.2 - 83.3 µin/in-°F

@Temperature 32.0 - 104 °F
1
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
CTE, linear, Parallel to Flow 130 - 150 µm/m-°C

@Temperature 0.000 - 40.0 °C
72.2 - 83.3 µin/in-°F

@Temperature 32.0 - 104 °F
ASTM D696
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.