Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 184 µm/m-°C @Temperature 20.0 °C |
102 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 487 Thermoplastic Polyurethane Desmopan 487 is a TPU on the basis of a special ester.Applications: Seals, gear wheels, shoe heels, engineering components in the automotive sector.Information provided by Bayer.As of 1 September 20.. |