Polymer Property : CTE, linear, Parallel to Flow = 21.4 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS
Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.