Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
21.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66
LNP* LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant.