Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 47.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.5 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |