Polymer Property : CTE, linear, Parallel to Flow = 26.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific)
Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require..
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI
LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature -30.0 - 100 °C
26.7 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP
SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East)
LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized.
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66
LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
26.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
26.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
CTE, linear, Parallel to Flow 48.0 µm/m-°C
26.7 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TC154 PA46 FR(17)
Thermal conductive material, Flame Retardant, Heat Stabilized
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
26.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
CTE, linear, Parallel to Flow 48.0 µm/m-°C
26.7 µin/in-°F
dry; ISO 11359-1/-2
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30
10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized