Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 28.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |