Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 56.3 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 56.4 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10 LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |