Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 414 µm/m-°C
230 µin/in-°F
ASTM D696
Techmer ES HiFill® PA12 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.