CTE, linear, Parallel to Flow 80.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL REN501 PPE+PS
Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only.
CTE, linear, Parallel to Flow 80.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL SE1X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications.