Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 45.3 µm/m-°C @Temperature -40.0 - 60.0 °C |
25.2 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 830R PBT (Asia Pacific) 30% glass filled, release grade, polyester alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |