CTE, linear, Parallel to Flow 92.4 µm/m-°C

@Temperature -30.0 - 30.0 °C
51.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT