CTE, linear, Parallel to Flow 97.0 µm/m-°C

@Temperature 20.0 °C
53.9 µin/in-°F

@Temperature 68.0 °F
Eastman Eastar DN007 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Parallel to Flow 97.0 µm/m-°C

@Temperature 20.0 °C
53.9 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® 556
Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoforming
CTE, linear, Parallel to Flow 97.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
53.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RI001 is a compound based on Nylon 66 resin containing Silicone.
CTE, linear, Parallel to Flow 97.0 µm/m-°C

@Temperature 20.0 °C
53.9 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnum™ 3490 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB..