Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.7 µm/m-°C

@Temperature 20.0 °C
31.5 µin/in-°F

@Temperature 68.0 °F
ASTM data
Styron CALIBREâ„¢ SF 7070 Polycarbonate, 7% Glass Reinforced Structural Foam Grade
CALIBRE® SF7070. is a 7% glass reinforced structural foam ignition resistant polycarbonate resin specially developed for injection molding processing. The CALIBRE 7070 resin provides a high flexu..