Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 133 µm/m-°C @Temperature -40.0 - 60.0 °C |
73.9 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl ENV85 PPE+PS (Asia Pacific) Low heat, flame retardant, extrusion grade PPO/HIPS alloy.Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region. |