Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature 0.000 - 100 °C |
42.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PN235 PPE+PS Plating grade, primarily automotive applications. |
|||
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature 0.000 - 100 °C |
42.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific) Plating grade, primarily automotive applications. |
|||
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN®-V 400T ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
CTE, linear, Parallel to Flow | 75.6 µm/m-°C @Temperature 20.0 °C |
42.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN®-V 420 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |