Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® R-FR 610 Polycarbonate/ABS Blend
(discontinued **) FR-recycled grades with 25% recycled content.Applications: Housings for office equipment, electrical engineering, computer sectors.Information provided by Bayer.As of 1 September 2015, Bayer Materia.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ASTM D696 |
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3000 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 97 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and hydrolysis resistance antimony-, chlorine- and bromine-free flame retardant.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade Flame retardant extrusion gradeVicat/B 120 temperature = 115 °Cgood extrusion and vacuum-forming behaviourUL-listing 94 V-0 (1.5 mm)halogen-free according to DIN VDE 0472-815glow wire temperature (.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 86 Polycarbonate/ABS Blend Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3001 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3010 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3012 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3040 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP CL002 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CL002 is a compound based on Polystyrene resin containing PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV006BS PP LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |