Polymer Property : CTE, linear, Parallel to Flow = 95.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature -40.0 - 40.0 °C
95.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 1103 PBT+PC
AUTOMOTIVE. Unreinforced, impact modified PBT+PC alloy. Excellent low temperature impact and chemical resistance. Range gray, black colors.
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature 20.0 °C
95.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ..
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature 20.0 °C
95.0 µin/in-°F

@Temperature 68.0 °F
ASTM D969
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro..
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature 20.0 °C
95.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod..