Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 800 °C | 1470 °F | ISO 7884-8 |
Schott GM31684 Dental Glass Remarks: High refractive index glass ceramicApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
Transformation Temperature, Tg | 800 °C | 1470 °F | ISO 7884-8 |
Schott GM31685 Dental Glass Remarks: Low refractive index glass ceramicApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCH.. |