Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 592 °C | 1100 °F | |
Schott N-BAK1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 592 °C | 1100 °F | |
Schott N-SF11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 592 °C | 1100 °F | |
Schott RG665 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |