Polymer Property : Transformation Temperature, Tg = 840 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 449 °C
840 °F
Mo-Sci Corporation WB-40-N White B Filter Glass
Applications: Lead-free NVIS White class B filter glass for white LED sources.Information provided by Mo-Sci Corporation.
Transformation Temperature, Tg 449 °C
840 °F
Mo-Sci Corporation YB-40-N Yellow B Filter Glass
Applications: Lead-free NVIS Yellow class B filter glass for white LED sources.Information provided by Mo-Sci Corporation.