Polymer Property : Clash Berg Stiffness Temperature = -25.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -25.0 °C
-13.0 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® HPG-6525 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..