Polymer Property : Clash Berg Stiffness Temperature = -44.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -42.2 °C
-44.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..