Clash Berg Stiffness Temperature -21.0 °C
-5.80 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (disco
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
Clash Berg Stiffness Temperature -21.0 °C
-5.80 °F
T-10000 Torsional stiffness ASTM D1043-72(1981)
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..