Polymer Property : Clash Berg Stiffness Temperature = -94.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature <= -70.0 °C
<= -94.0 °F
at 930 MPa; ASTM D1043
Eastman Neostar FN005 Elastomer
Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough..
Clash Berg Stiffness Temperature <= -70.0 °C
<= -94.0 °F
at 930 MPa; ASTM D1043
Eastman Neostar FN006 Elastomer
Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and ..
Clash Berg Stiffness Temperature <= -70.0 °C
<= -94.0 °F
at 930 MPa; ASTM D1043
Eastman Neostar FN007 Elastomer
Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol..